Abstract:Erosion wear is the main abrasion to the jet element of complete fluidic sprinkler.In order to study the effects on the reliability of complete fluidic sprinkler by erosion wear,three failure indexes about complete fluidic sprinkler were defined as droplet diameter of the distal end of sprinkler,stepping frequency and stepping angle.A wear and tear test was conducted under the mass concentration of 1%,2% and 3%.The hydraulic performances were studied in the test,including the changing rules with the time of flux of nozzle,the flux of signal tube and the diameter of droplet at the end of spray.The test results indicate that the extent of the change of hydraulic performance,droplet diameter of the distal end of sprinkler,stepping frequency and stepping angle,increase with the mass concentration,while the effects on hydraulic performance decrease gradually with the mass concentration.Signal Tube 1 is the wearing terrain,so it should be made with wear resistant material to increase the reliability of sprinkler.
[1] 李红,任志远,谢福祺.全射流喷头的磨损试验[J].农业机械学报,2006,37(12):105-108[2] Yazar A.Evaporation and drift losses from sprinkler irrigation systems under various operating conditions[J].Agricultural Water Management,1984(8):439-449[3] 邓军,杨永全,沈焕荣.水流含沙量对磨蚀的影响[J].泥沙研究,2000(4):65-68[4] 朱兴业,袁寿其,李红.全射流喷头的原理及实验研究[J].排灌机械,2005,23(2):23-26[5] 黄志斌,张世芳.自反馈式射流喷头的设计[J].江苏工学院学报,1985(2):35-38[6] 董刚,张九渊.固体粒子冲蚀磨损研究进展[J].材料科学与工程,2003,21(2):307-312[7] Tilly G P.Treatise on material science and technology[J].Wear,1979,53:287-317[8] 中国机械工程学会材料分会.磨损失效分析[M].北京:机械工业出版社,1991[9] 陈大雕,林中卉.喷灌技术[M].北京:中国科学技术出版社,1992[10] 李世英.喷灌喷头理论与设计[M].北京:兵器工业出版社,1995[11] Edling R J.Kinetic energy.evaporation and wind drift of droplets from low pressure irrigation nozzles[J].Transactions of the ASME,1985,28:1543-1550